Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer

Key Words: LLDPE

Material Notes:
Low Density, Linear Polyethylene Film Resin

Customer Benefits: This unique broad molecular weight distribution resin has a wide processing window and produces film with an excellent combination of toughness and tensile. D252/257 may be used straight, in blends, or coextruded with HMW-HDPE, LLDPE, and LDPE. It is especially well suited in blends with LLDPE to increase melt strength and processing rate of LLDPE. In thick gauge heavy duty applications, the benefit of the high molecular weight tail is seen in puncture resistance. Processing is excellent on many types of equipment and under a variety of conditions, including high stalk. Meets FDA regulations for food packaging below cooking temperatures. D256 contains premium stabilizer.

Applications: Heavy wall bags

Property Comments: HDPE line, 4:1 BUR, .035" gap, 8" die, 56" FLH, 240 lbs/hr, 420°F

Data provided by Chevron Phillips Chemical Company LP.

Available Properties
  • Density
  • Melt Flow
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Elmendorf Tear Strength MD
  • Elmendorf Tear Strength TD
  • Dart Drop Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。