Chevron Phillips Marlex® HHM TR-130 Medium Density Polyethylene, Medium Molecular Weight Film Resin
Subcategory: Polyethylene; Thermoplastic; MDPE; Polymer
Key Words: MDPE
Material Notes: Medium Density, Medium Molecular Weight Film Resin Customer Benefits: This medium density resin provides an excellent overall balance of tensile, impact, and tear properties in thin film. It is well suited for merchandise, produce, and trash bags. Processing performance is excellent on high stalk lines. HHM TR-130 meets FDA regulations for food packaging. Applications: Merchandise bags, T-Shirts bags, trash bags Property Comments: HDPE line, 4:1 BUR, .035" gap, 8" die, 56" FLH, 240 lbs/hr, 420°F Data provided by Chevron Phillips Chemical Company LP.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|