Chevron Phillips Marlex® HMN 55180 High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: HDPE
Material Notes: High Density Polyethylene Customer Benefits: This resin is a narrow molecular weight distribution copolymer with easy processing characteristics and excellent toughness properties. This product displays excellent color, low odor, and processing stability. It is generally recommended for housewares, containers, and cap closure applications. Applications: Tote bags, housewares, food containers Property Comments: Physical Properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Data provided by Chevron Phillips Chemical Company LP.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|