Chevron Phillips Oxygen-Scavenging Polymer OSP500R EMCM Resin

 

Subcategory: Thermoplastic

Material Notes:
Ethylene Methyl Acrylate Cyclohexene Methyl Acrylate (EMCM) is a polymer that will oxidize but not degrade. CHMA content 14.0% (wt.). Primary antioxidant 150 ppm. Oxygen capacity 65 cc/gm.

OSP500R is designed for use in coextruded blown film applications at gauges of 0.25 mil to 1.5 mil of a non-food contact layer.  This resin should be blended with one of the Catalyst/Photoinitiator Masterbatches in order to properly activate the oxygen scavenging mechanism. Typical blend ratios range from 95:5 to 85:15 (EMCM/MB) with 90:10 being the recommended blend ratio for most applications. Recommended extrusion melt temperatures range from 250°F to 400°F when blended with OSP100M Masterbatch. Higher melt temperature extrusion of up to 550°F is possible when blending with OSP150M.

OSP polymers are used in packaging for O2-sensitive applications from food to electronics. Packaging produced with OSP polymers can extend product life, eliminating waste and providing greater distribution flexibility. Oxygen scavenging rates and capacities are influenced significantly by UV activation dose, use conditions such as storage temperatures, and initial package oxygen content.

Information provided by Chevron Phillips Chemical Company.

Available Properties
  • Density
  • Melt Flow
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。