Chevron Phillips Oxygen-Scavenging Polymer OSP150M Catalyst & Photoinitiator Masterbatch
Subcategory: Thermoplastic
Material Notes: Cobalt content 1.0 % (wt.). Photoinitiator content 1.0% (wt.). Primary antioxidant 5000 ppm. OSP150M is a high-temperature use catalyst/photoinitiator masterbatch designed for use in extrusion coating and cast film applications. This resin should be blended with one of the EMCM resins in order to properly activate the oxygen scavenging mechanism. Typical blend ratios range from 95:5 to 85:15 (EMCM/MB) with 90:10 being the recommended blend ratio for most applications. Recommended extrusion melt temperatures range from 450°F to 550°F. OSP polymers are used in packaging for O2-sensitive applications from food to electronics. Packaging produced with OSP polymers can extend product life, eliminating waste and providing greater distribution flexibility. Oxygen scavenging rates and capacities are influenced significantly by UV activation dose, use conditions such as storage temperatures, and initial package oxygen content. Information provided by Chevron Phillips Chemical Company.
| Available Properties |
- Density
- Melt Flow
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|