Chevron Phillips mPact™ D350 m-LLDPE Linear Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Low Density Polyethylene Customer Benefits: This medium density metallocene polyethylene film resins combines the benefits of .933 density (modulus, barrier, c.o.f.) with the clarity of mLLDPE. Applications: Merchandise bags, liners Property Comments: LLDPE line, 2.5:1 BUR, .08" diegap, 8" die, 56" FLH, 250 lbs/hr, 400°F Data provided by Chevron Phillips Chemical Company LP.