Chevron Phillips mPact™ D449 HDPE Blown Film Resin
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Key Words: High Density Polyethylene
Material Notes: Resin Type: High density, hexene copolymer Characteristics: excellent clarity, high gloss, good modulus, process with LLDPE setup, optimum clarity when used as an individual layer. Applications: overwraps, FFS packaging, food packaging, coextruded converter films Recommended processing conditions: 8.89 cm extruder. 30:1 L/D extruder. 20.32 die and 80 mil gap at 250 pph with a melt temperature of 400-430°F. Data provided by Chevron Phillips Chemical Company, LP.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Haze
- Gloss
- Processing Temperature
- Die Opening
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|