Phillips Sumika Marlex® AHX-230 Polypropylene Impact Copolymer

 

Subcategory: Polypropylene; Thermoplastic

Key Words: PP

Material Notes:
Polypropylene Impact Copolymer, Heat Stabilized

Applications: Formulated for automotive interior trim, durables, housewares, and consumer products

Comments: Meets FDA Regulation 21 CFR 177.1520 and may be safely used as articles for use in contact with food except for articles used for packing or holding food during cooking. UL yellow card RTI of 65°C and a flame rating of UL94HB, these apply to natural color at a minimum thickness of 0.058".

The nominal properties reported herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Data provided by Phillips Sumika Polypropylene Company (PSPC).

Available Properties
  • Density
  • Melt Flow
  • Hardness, Rockwell R
  • Tensile Strength, Yield
  • Flexural Modulus
  • Izod Impact, Notched
  • Izod Impact, Notched, Low Temp
  • Impact Test
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。