Phillips Sumika Marlex® BPC-70 Polypropylene Talc-Filled Impact Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: PP
Material Notes: Polypropylene Talc-Filled Impact Copolymer Applications: Formulated for Automotive Interior Door Panel Applications The nominal properties reported herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes. Data provided by Phillips Sumika Polypropylene Company (PSPC).
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched, Low Temp (ISO)
- Izod Impact Resistance
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|