Phillips Sumika Marlex® HGV-180 Polypropylene Homopolymer, General Purpose Fiber Grade, low gas fading
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes:
Applications: Bulked Continuous Filament, Craft Yarn, Nonwoven Fabrics Comments: Meets FDA Regulation 21 CFR 177.1520 and is suitable for food packaging at temperatures not exceeding 212°F (100C). Information provided by Phillips Sumika Polypropylene Company (PSPC).
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |