Phillips Sumika Marlex® HGX-030-01 Polypropylene Homopolymer, Fiber Grade
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Polypropylene Homopolymer, Fiber Grade, Low Water Carryover Applications: Formulated for woven industrial fabric and bags, woven carpet backing, woven bags, woven geotextile fabrics, rope and cordage Comments: Meets FDA Regulation 21 CFR 177.1520 and is suitable for food packaging applications The nominal properties reported herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes. Data provided by Phillips Sumika Polypropylene Company (PSPC).
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|