Phillips Sumika Marlex® RLC-120 Polypropylene Random Copolymer, Clarified polypropylene, antistatic
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes:
Applications: Food containers; large storage boxes; deli containers; ISBM bottles Comments: Meets FDA Regulation 21 CFR 177.1520 and is suitable for food packaging applications. Information provided by Phillips Sumika Polypropylene Company (PSPC).
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|