Phillips Sumika Marlex® RLN-350 Polypropylene Random Copolymer, Antistatic
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Polypropylene Random Copolymer, Antistatic, Nucleated, Controlled Rheology Applications: Formulated for toys, flower pots, thin wall containers, video cassette boxes, and promotional drink cups Comments: Meets FDA Regulation 21 CFR 177.1520 and is suitable for food packaging applications. Listed in the Drug Master File. UL Listed, 1.5 mm thick, natural, RTI 65°C, Flame Rating 94HB The nominal properties reported herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes. Data provided by Phillips Sumika Polypropylene Company (PSPC).
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|