Chevron Phillips 6335B LLDPE Cast/Blown Film Resin, Butene Copolymer
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Resin Type: Butene Copolymer, Medium Slip Version of 6335 Characteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applications, Low COF. Slip 1000 ppm. Applications:Bakery Films, Coextrusions Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.1016 cm. Film properties below based on film thickness of 31.8 µm. Data provided by Chevron Chemical.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|