Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Resin Type: Hexene Copolymer, Cast/Blown Film Resin Characteristics: Good Drawdown, Can be used in blown or cast applications Applications:Stretch Wrap, Coextrusions Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.064 cm. Film properties below based on film thickness of 20 µm. Data provided by Chevron Chemical.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |