Chevron Phillips HiD® 9018 HDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 53600 Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage Resistance Applications:Housewares, Automotive, Tamper Evident Screw Caps for Milk Bottles, Pails (1-2 gallon), Toys, Small Containers for Building Compounds Data provided by Chevron Chemical.
| Available Properties |
- Density
- Apparent Bulk Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |