Chevron Phillips HiD® 9062 HDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600 Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage Resistance Applications:Thin Wall Food Containers, Stadium Cups Data provided by Chevron Chemical.
| Available Properties |
- Density
- Apparent Bulk Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
|
|
|
|