Chevron Phillips HiD® 9406 HDPE Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Resin Type: Linear Copolymer; Blow Molding Resin Characteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good Stress Crack Resistance Applications:"Hard to Hold" Industrial Chemicals, Automotive Parts, Edible Oil Packaging, Large Trash Cans Data provided by Chevron Chemical.
| Available Properties |
- Density
- Apparent Bulk Density
- Melt Flow
|
|
|
|