Chevron Phillips HiD® 9410 HDPE Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Resin Type: Linear Copolymer; Blow Molding Resin Characteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good Trimability Applications:Pharmaceutical Applications, Personal Care Products, Household-Industrial Chemical Containers, Sheet and Vacuum Forming. Burn Rate <5 cm/min. Data provided by Chevron Chemical.
| Available Properties |
- Density
- Apparent Bulk Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|