Chevron Phillips HiD® 9502/HiD® 9503 with Antistat HDPE Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Resin Type: Linear Copolymer; Blow Molding Resin Characteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Excellent ESCR, High Melt Strength, Good Impact Resistance, Good Parison Uniformity, Good Trimability Applications:Hard to Hold Chemicals, Household-Industrial Chemical Containers, Detergents. Burn Rate <5 cm/min. Data provided by Chevron Chemical.
| Available Properties |
- Density
- Apparent Bulk Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|