Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet Resin
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Material Notes: Resin Type: ASTM D 4976 Classification: PE 235, A 54502 Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Stress Crack Resistance Film properties below based on film thickness of 25.4 µm. Data provided by Chevron Chemical.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|