Chevron Phillips PE 4610 LDPE High Clarity, Bakery Packaging Film Resin
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Low Density Polyethylene
Material Notes: Resin Type: Homopolymer Characteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal Characteristics Applications:Bakery Film, Sanitary Film Packaging Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0508 cm. Film properties below based on film thickness of 31.8 µm. Data provided by Chevron Chemical.
| Available Properties |
- Density
- Melt Flow
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Dart Drop
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|