Chevron Phillips PE 5036 LDPE High Clarity, Impact Film Resin
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Low Density Polyethylene
Material Notes: Resin Type: Homopolymer; for General Purpose Packaging Characteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent Processability Applications:Frozen Food Packaging, Heavy Produce Bags, Dry Goods Packaging Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Film properties below based on film thickness of 31.8 µm. Data provided by Chevron Chemical.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Dart Drop
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|