Eastman PE 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; LDPE; Polymer
Key Words: Ethylene Vinyl Acetate; EVA; Eastman EVA
Material Notes: Resin Type: VA Copolymer Characteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strength Applications:Laminations, Heavy produce and skin packaging, Frozen food packaging Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1. Film properties below based on film thickness of 31.8 µm. Data provided by Chevron Chemical, 1999. Chevron sold its EVA product line to Eastman Chemical in 1999.
| Available Properties |
- Density
- Melt Flow
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Dart Drop
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|