Eastman SP 1205 EMAC® Ethylene-Methyl Acrylate Copolymer
Subcategory: Ethylene Methyl Acrylate; Thermoplastic
Key Words: Eastman EMAC
Material Notes: 20% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing up to 600°F, Non-Corrosive at Extrusion Temperatures, FDA Clearance for Packaging of Most Foods - including Aseptic Packaging, No FDA thickness limitation Applications:Coatings & Laminations: Higher Neck-In but Similar Drawdown vs. LDPE Extrusion Coating Grades, Excellent Heat Seal Response at Low Seal Temperatures, Adheres Very Well to Non-Porous Substrates such as OPP, PVDC Coated Substrates, and Polyester, Adheres well to Porous Substrates such as Paper and Paperboard; Compounding: Impact Modification, Compatibilizer; Film: Tie Layers for LDPE, LLDPE, HDPE, PET, PP, PVDC, Ionomer, EVA, EAA, PVC (Rigid), PC Data provided by Chevron Chemical. Chevron sold its EMAC® and EBAC® product lines to Eastman Chemical in 1999.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|