Eastman SP 1802 EBAC® Ethylene-Butyl Acrylate Copolymer
Subcategory: Ethylene Butyl Acrylate; Thermoplastic
Key Words: Eastman EBAC
Material Notes: 18% Butyl Acrylate Content. Characteristics: Processing Temperature Range: 350-600°F, Less Crystalline and Softer than Polyethylene, Non-Corrosive at Extrusion Temperatures, Excellent Thermal Stability Over the Full Processing Temperature Range, Contains No Slip and Antiblock Additives Applications:Film: Processable on Standard LDPE Film Lines, Excellent Heat Seal Response at Low Temperatures, Melt Strength to Produce 10 mil and Thicker Blown Films, Excellent Toughness and Creep Resistance; Compounding: Impact Modification, Compatibilizer; Coextrusion: Excellent Coextrusion Tie Layer for LDPE, LLDPE, HDPE, PP, EVA, EEA, Ionomer, PET, PC, PVDC, and rigid PVC, Broad Operating Temperature Range facilitates Viscosity Matching Data provided by Chevron Chemical. Chevron sold its EMAC® and EBAC® product lines to Eastman Chemical in 1999.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Melting Point
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|