Chevron Phillips HiD® 9330T HDPE Natural Pipe Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Resin Type: Gas Phase Linear Hexene Copolymer ASTM D 4976 Classification: PE 235, A 54607 ASTM D3350 Classification: 335540A Applications: Base resin for use in utility and conduit pipe applications. Data provided by Chevron Chemical.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|