Chevron Phillips 7120S Linear low density polyethylene blown film resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Resin Type: linear low density polyethylene, hexene copolymer, melt index - 2.0 g/10 min., density - 0.918 g/cc, cast/blown film resin Characteristics: good drawdown, can be used in blown or cast applications Applications: stretch wrap, coextrusions Natural Color. Film properties below based on thickness of 0.02 mm. Extruder 6.35 cm. Screw L/D ratio 24:1. Die opening 0.064 cm. Information provided by Chevron Phillips Chemical Company
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|