Chevron Phillips 7109L Linear low density polyethylene blown film resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Resin Type: linear low density, hexene copolymer, high antiblock version of 7109, blown film resin Characteristics: good stiffness at thin gauges, good drawdown, low COF, can be used straight or blended with LDPE or HDPE Applications: industrial liners, garment bags, carrier bags, coextrusions Natural Color. 6500 ppm Antiblock. Film properties below based on thickness of 0.0318 mm. Extruder 6.35 cm. Screw L/D ratio 24:1. Die opening 0.1905 cm. Blow-Up Ratio 2:1. Information provided by Chevron Phillips Chemical Company
| Available Properties |
- Density
- Melt Flow
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Dart Drop
- Dart Drop Test
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|