Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes:
Resin Type: linear copolymer Characteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C Classification Type I, Class H, Grades (1-5), Category 5. Meets FDA Regulation 21CFR 177.1520. Some restrictions apply when containing an antistatic additive. Applications: industrial blow molding, automotive parts, toys, large trash cans, ice chests and coolers Information provided by Chevron Phillips Chemical Company.
| Available Properties |
- Density
- Apparent Bulk Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|