Chevron Phillips LX8124 HDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes:
Resin Type: linear copolymer; ASTM D4976 Classification: PE 231, A 52600 Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, excellent shrinkage resistance Applications: thin wall food containers, stadium cups Information provided by Chevron Phillips Chemical Company.