Chevron Phillips PE 1013 LDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; LDPE
Key Words: Low Density Polyethylene
Material Notes:
Resin Type: Low density, polyethylene, high speed resin Characteristics: excellent processability, high temperature extrusion stability, good draw down resin. Federal specification LP390C Classification Type I, Class H, Grades (1-5), Category 5. Meets FDA Regulation 21CFR 177.1520. Applications: food packaging, laminations Translucent to clear. Information provided by Chevron Phillips Chemical Company.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,