Chevron Phillips HiD® 9656 HDPE Blown Film Resin
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Key Words: High Density Polyethylene
Material Notes: Resin Type: high density, linear polyethylene. Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPE Applications: notion and millinery bags, multi-wall liners, coextrusions Recommended processing conditions: Die Gap 0.030-0.050 in. Melt Temperature 400°F. Data provided by Chevron Phillips Chemical Company, LP.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Thickness
- Melt Flow
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Processing Temperature
- Die Opening
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|