Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Linear Low Density Polyethylene
Material Notes:
Resin Type: processing aid additive Characteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blended with LDPE or HDPE Applications: thick or thin film applications where excellent toughness and abuse resistance, hot-tack and heat seal properties are required Natural Color Slip: 0 ppm Antiblock: 0 ppm. Recommended processing conditions: 6.35 cm extruder. 24:1 screw L/D ratio. 0.203 cm die opening. Melt temperature 232°C. Blow up ratio 2.5:1. Output rate 8.0 lb/hr/in die cir. Hot-Tack Initiation Temperature: °C Ultimate Hot-Tack Strength: 3 N Heat Seal Initiation Temperature at 0.5 lb.: 95°C Ultimate Heat Seal Strength: N. Film properties based on thickness of 0.0318 mm. Information provided by Chevron Phillips Chemical Company.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Dart Drop Test
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|