Chevron Phillips Ryton® R-4 Polyphenylene Sulfide Compound
Subcategory: Polyphenylene Sulfide; Thermoplastic
Key Words: PPS
Material Notes: Natural Color Polyphenylene Sulfide Compound Ryton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at elevated temperatures. Comments: Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C; ASTM Values Converted to SI Units Data provided by Chevron Phillips Chemical Company LP.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Deformation
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Poissons Ratio
- Fatigue Strength
- Shear Strength
- Izod Impact, Notched
- Izod Impact, Unnotched
- Izod Impact, Notched, Low Temp
- Coefficient of Friction
- Coefficient of Friction, Static
- Taber Abrasion, mg/1000 Cycles
- Izod Impact, Unnotched @ -40°C
- Electrical Resistivity
- Surface Resistance
- Insulation Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|