Chevron Phillips Ryton® P-6 Polyphenylene Sulfide Coating Resin
Subcategory: Polyphenylene Sulfide; Thermoplastic
Key Words: PPS
Material Notes: Tan Color Polyphenylene Sulfide Coating Resin Ryton® P-6 is used for coatings and is a finely divided powder having a modest molecular weight and high melt flow. The powder (neat or mixed with other components) may be applied using slurry or electrical spray methods, and then fused and cured (cross-linking and chain extension) at temperatures from 600°F (316°C) to 800°F (427°C) to form high temperature, non-stick, corrosion resistant coatings. For further information on Ryton® PPS Coatings, request Ryton® TMM-275. 0.8 wt % Ash. Particle size: 95 wt % passing 35 mesh. 90 wt % passing 60 mesh. Data provided by Chevron Phillips Chemical Company LP.
| Available Properties |
- Melt Flow
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|