Chevron Phillips Ryton® GR01 Polyphenylene Sulfide Resin
Subcategory: Polyphenylene Sulfide; Thermoplastic
Key Words: PPS
Material Notes: Off White Polyphenylene Sulfide Resin Ryton® GR01 is a finely divided powder. Ryton® PPS exhibits excellent thermal stability and chemical resistance and is suitable for a variety of applications including compounds, coatings, film, and fiber. 0.6 wt % Ash. Particle size: 65 wt % passing 35 mesh. 50 wt % passing 60 mesh. Data provided by Chevron Phillips Chemical Company LP.
|
|
|