Chevron Phillips Marlex® C514 HDPE Pipe and Corrugated Extrusion Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Characteristics: - Good melt strength
- Good pipe stiffness
- Good ESCR
Applications: - Culverts
- Storm sewers
- Land drainage
Information provided by Chevron Phillips.