Chevron Phillips Marlex® 9005 LDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: Resin Type: Hexene Copolymer Characteristics: - Moderate flow
- Excellent impact strength
- Excellent ESCR
- Good warpage resistance
Applications: - Industrial parts
- Seats
- Food and household containers
- Agricultural parts
Information provided by Chevron Phillips.
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |