Chevron Phillips Ryton® R10-110BL Glass and Mineral Filled Polyphenylene Sulfide Compound
Subcategory: Polyphenylene Sulfide; Thermoplastic; Polymer
Material Notes: Description: Ryton® R10-110BL is a glass and mineral filled polyphenylene sulfide compound that provides a good combination of mechanical and electrical properties with the inherent cost savings of thermoplastics. Comments: Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C Information provided by Chevron Phillips.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched (ISO)
- Volume Resistivity
- Insulation Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- CTE, linear 100°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|