Phillips Sumika Marlex® EX01D Polypropylene; Homopolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Meets FDA regulation 21 CFR 177.1520 and is suitable for food packaging applications.
Material Notes: Modified polypropylene homopolymer, premium nonwoven/extrusion coating grade. Applications: Nonwoven spunbonded fabrics, nonwoven melt blown fabrics, and extrusion coating. Information provided by Phillips