Phillips Sumika Marlex® RGC-020-04 Polypropylene; Random Copolymers
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Meets FDA regulations 21 CFR 177.1520 (c)3.1a and (c)3.2a, and may safely be used for articles used in packing or holding food during cooking.
Material Notes: Polypropylene random copolymer, clarified. Applications: Syrup and large juice bottles, toiletry and cosmetic bottles. Information provided by Phillips
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Haze
- Transmission, Visible
|
|
|
|