Phillips Sumika Marlex® AGM-010 Polypropylene; Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Meets FDA regulation CFR 177.1520 and may safely be used for articles in contact with food except for articles used for packing or holding food during cooking.
Material Notes: Polypropylene impact copolymer, cold temperature impact resistant. Applications: Thermoformed parts, blow molded parts, and profile extrusion. Information provided by Phillips
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Back Pressure
- Manifold Temperature °F
- Parison Temperature °F
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|