Phillips Sumika Marlex® ALN-070 Polypropylene; Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Polypropylene impact copolymer, high impact strength, lubricated. Applications: - Pallets
- Industrial bins
- Bulk containers
- Returnable packaging
Information provided by Phillips
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Storage Temperature
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Back Pressure
- Screw Speed %
- Suggested Shot Size %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|