Chevron Phillips Chemical Co. Marlex® 9514H Polyethylene; HDPE
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: This resin meets these specifications: - ASTM D4976 - PE 235
- FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)
Material Notes: High density polyethylene. This gas phase, high molecular weight hexene copolymer is tailored for lightweight blow molded applications that: - Require excellent stiffness to ESCR ratio
- Require good melt strength
- Are durable and recyclable for sustainability
Applications: Typical blow molded applications for 9514H include: - Household and industrial chemical containers
- Large parts
Information provided by Phillips
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Index of Compound
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|