Chevron Phillips Chemical Co. Marlex® H516 Polyethylene; HDPE
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: This compound meets or exceeds: - ASTM D4976 - PE 235
- ASTM D3350, class 445574C and 445576C
- NSF Standards 14 and 61 for potable water
- PPI designations PE 4710 and PE 100
Material Notes: High density polyethylene compound. This high performance PE 100 HDPE compound is tailored for the demanding requirements of pressure pipe applications that require: - Excellent long-term hoop strength
- Superb resistance to slow-crack growth
- Exceptional resistance to rapid-crack propagation
- Outstanding low-temperature toughness
Additional information: Yellow version also available.Applications: Typical pipe applications for H516 include: - Gas distribution
- Potable water
- Industrial applications
Information provided by Phillips
| Available Properties |
- Density
- PENT
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Hydrostatic Design Basis @ 73°F
- Hydrostatic Design Basis @ 140°F Mpa
- Hydrostatic Strength, hour
- Notched Pipe Test @ 4.6 MPa hour
- Rapid Crack Propagation bar
- Required Minimum Strength MPa
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|