Chevron Phillips Chemical Co. Marlex® C101 Polyethylene; Enhanced
Subcategory: Polyethylene; Thermoplastic; LLDPE
Close Analogs: This resin meets these specifications: - ASTM D4976 - PE 213
- FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)
Material Notes: Metallocene linear low density polyethylene. This linear low density, hexene copolymer is tailored for blow molded containers that require: - High gloss
- Good clarity
- Excellent ESCR
Applications: Typical blow molded applications for C101 include: - Glossy multilayer bottles
- Squeezable bottles
Information provided by Phillips
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Index of Compound
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|