Chevron Phillips Chemical Co. MarFlex® ER3343 Polyethylene; Masterbatch
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Metallocene polyethylene slip masterbatch. This erucamide slip concentrate with its mLLDPE carrier is tailored for use with mPact™ resins in blown film applications that require: - Reduced COF
- Excellent optics
- Excellent strength
Applications: Typical blown film applications include: - Use with MarFlex™ D139 and MarFlex™ D143
- Use as needed to obtain desired slip level and COF
- May also be used with conventional LLDPE
Information provided by Phillips
| Available Properties |
- Density
- Melt Index of Compound
- Slip
|
|
|
|
| Property Data |