Chevron Phillips Ryton® R-7-121NA Polyphenylene Sulfide Resin
Subcategory: Polyphenylene Sulfide; Thermoplastic
Close Analogs: Measured on 102mm x 102mm x 3.2 mm plaques, edge gated.
Material Notes: Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional molding equipment.Information provided by Chevron Phillips
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Storage Temperature
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched (ISO)
- Volume Resistivity
- Insulation Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- Flammability, UL94
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|