Chevron Phillips MC3650 Crystal Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: General purpose crystal polystyrene.Applications: - Housewares
- Consumer containers, vials, jars, etc.
- Disposable cutlery
- Injection molded drink cups
Features:- Easy filling of thin-walled parts
- Exceptional mold release
- Excellent clarity with slight blue tint
- Improved cycle times in hard to fill parts
- Good toughness
Information provided by Chevron Phillips
| Available Properties |
- Specific Gravity
- Bulk Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|